Modeling of galvanostatic charge and discharge of the lithium/polymer/insertion cell
M Doyle, TF Fuller, J Newman
Journal of the Electrochemical society 140 (6), 1526, 1993
46181993
Simulation and optimization of the dual lithium ion insertion cell
TF Fuller, M Doyle, J Newman
Journal of the electrochemical society 141 (1), 1, 1994
23431994
A critical review of thermal issues in lithium-ion batteries
TM Bandhauer, S Garimella, TF Fuller
Journal of the electrochemical society 158 (3), R1, 2011
22392011
Toward efficient binders for Li-ion battery Si-based anodes: polyacrylic acid
A Magasinski, B Zdyrko, I Kovalenko, B Hertzberg, R Burtovyy, ...
ACS applied materials & interfaces 2 (11), 3004-3010, 2010
11842010
Water and thermal management in solid‐polymer‐electrolyte fuel cells
TF Fuller, J Newman
Journal of the Electrochemical Society 140 (5), 1218, 1993
10901993
A historical perspective of fuel cell technology in the 20th century
ML Perry, TF Fuller
Journal-Electrochemical Society 149 (7), S59-S67, 2002
7282002
The importance of the lithium ion transference number in lithium/polymer cells
M Doyle, TF Fuller, J Newman
Electrochimica Acta 39 (13), 2073-2081, 1994
6701994
Relaxation phenomena in lithium‐ion‐insertion cells
TF Fuller, M Doyle, J Newman
Journal of the Electrochemical Society 141 (4), 982, 1994
5801994
Carbon as catalyst and support for electrochemical energy conversion
P Trogadas, TF Fuller, P Strasser
Carbon 75, 5-42, 2014
5792014
Experimental determination of the transport number of water in Nafion 117 membrane
TF Fuller, J Newman
Journal of the Electrochemical Society 139 (5), 1332, 1992
3821992
The measurement of a complete set of transport properties for a concentrated solid polymer electrolyte solution
Y Ma, M Doyle, TF Fuller, MM Doeff, LC De Jonghe, J Newman
Journal of the Electrochemical Society 142 (6), 1859, 1995
3701995
PEM fuel cell Pt∕ C dissolution and deposition in nafion electrolyte
W Bi, GE Gray, TF Fuller
Electrochemical and solid-state letters 10 (5), B101, 2007
3132007
Towards ultrathick battery electrodes: Aligned carbon nanotube–enabled architecture
K Evanoff, J Khan, AA Balandin, A Magasinski, WJ Ready, TF Fuller, ...
Advanced Materials 24 (4), 533-537, 2012
2982012
XPS investigation of Nafion® membrane degradation
C Chen, G Levitin, DW Hess, TF Fuller
Journal of Power Sources 169 (2), 288-295, 2007
2912007
Hierarchically structured nanomaterials for electrochemical energy conversion
P Trogadas, V Ramani, P Strasser, TF Fuller, MO Coppens
Angewandte Chemie International Edition 55 (1), 122-148, 2016
2582016
Electrochemical engineering
TF Fuller, JN Harb
John Wiley & Sons, 2018
2332018
Effects of dissolved transition metals on the electrochemical performance and SEI growth in lithium-ion batteries
T Joshi, KS Eom, G Yushin, TF Fuller
Journal of the electrochemical society 161 (12), A1915, 2014
2172014
Analysis of lithium insertion/deinsertion in a silicon electrode particle at room temperature
R Chandrasekaran, A Magasinski, G Yushin, TF Fuller
Journal of the Electrochemical Society 157 (10), A1139, 2010
2102010
Temperature effects on PEM fuel cells Pt/C catalyst degradation
W Bi, T Fuller
ECS Transactions 11 (1), 1235, 2007
2002007
The effect of humidity on the degradation of Nafion® membrane
C Chen, TF Fuller
Polymer Degradation and Stability 94 (9), 1436-1447, 2009
1972009