Critical crack-healing condition for SiC whisker reinforced alumina under stress
W Nakao, M Ono, SK Lee, K Takahashi, K Ando
Journal of the European Ceramic Society 25 (16), 3649-3655, 2005
952005
Strength recovery behavior of machined Al2O3/SiC nano-composite ceramics by crack-healing
T Osada, W Nakao, K Takahashi, K Ando, S Saito
Journal of the European Ceramic Society 27 (10), 3261-3267, 2007
932007
Kinetics of self‐crack‐healing of alumina/silicon carbide composite including oxygen partial pressure effect
T Osada, W Nakao, K Takahashi, K Ando
Journal of the American Ceramic Society 92 (4), 864-869, 2009
772009
Self‐crack‐healing behavior of mullite/SiC particle/SiC whisker multi‐composites and potential use for ceramic springs
W Nakao, S Mori, J Nakamura, K Takahashi, K Ando, M Yokouchi
Journal of the American Ceramic Society 89 (4), 1352-1357, 2006
752006
A novel design approach for self-crack-healing structural ceramics with 3D networks of healing activator
T Osada, K Kamoda, M Mitome, T Hara, T Abe, Y Tamagawa, W Nakao, ...
Scientific reports 7 (1), 17853, 2017
722017
Crack-healing behaviour of mullite/SiC/Y2O3 composites and its application to the structural integrity of machined components
SK Lee, M Ono, W Nakao, K Takahashi, K Ando
Journal of the European Ceramic Society 25 (15), 3495-3502, 2005
632005
On the use of TiC as high-temperature healing particles in alumina based composites
S Yoshioka, L Boatemaa, S van der Zwaag, W Nakao, WG Sloof
Journal of the European Ceramic Society 36 (16), 4155-4162, 2016
532016
Finite element analysis of the damage and healing behavior of self-healing ceramic materials
S Ozaki, T Osada, W Nakao
International Journal of Solids and Structures 100, 307-318, 2016
532016
Enhancement of the self-healing ability in oxidation induced self-healing ceramic by modifying the healing agent
W Nakao, S Abe
Smart materials and structures 21 (2), 025002, 2012
532012
Self-healing of surface cracks in structural ceramics
W Nakao, K Takahashi, K Ando
Self-healing Materials 6, 183-217, 2009
522009
A new methodology to guarantee the structural integrity of Al2O3/SiC composite using crack healing and a proof test
M Ono, W Nakao, K Takahashi, M Nakatani, K Ando
Fatigue & fracture of engineering materials & structures 30 (7), 599-607, 2007
522007
New synthetic method of forming aluminum oxynitride by plasma arc melting
H Fukuyama, W Nakao, M Susa, K Nagata
Journal of the American Ceramic Society 82 (6), 1381-1387, 1999
461999
Single crystalline aluminum nitride film, method of forming the same, base substrate for group III element nitride film, light emitting device and surface acoustic wave device
H Fukuyama, K Nagata, W Nakao
US Patent 6,744,076, 2004
452004
Finite element analysis of fracture statistics of ceramics: effects of grain size and pore size distributions
S Ozaki, Y Aoki, T Osada, K Takeo, W Nakao
Journal of the American Ceramic Society 101 (7), 3191-3204, 2018
432018
Gibbs Energy Change of Carbothermal Nitridation Reaction of Al2O3 to Form AlN and Reassessment of Thermochemical Properties of AlN
W Nakao, H Fukuyama, K Nagata
Journal of the American Ceramic Society 85 (4), 889-896, 2002
412002
Threshold stress during crack-healing treatment of structural ceramics having the crack-healing ability
W Nakao, K Takahashi, K Ando
Materials letters 61 (13), 2711-2713, 2007
372007
Methodology for evaluating self-healing agent of structural ceramics
S Yoshioka, W Nakao
Journal of Intelligent Material Systems and Structures 26 (11), 1395-1403, 2015
322015
Experimental evaluation of domain wall dynamics by Barkhausen noise analysis in Fe30Co70 magnetostrictive alloy wire
T Yamazaki, Y Furuya, W Nakao
Journal of Magnetism and Magnetic Materials 475, 240-248, 2019
302019
Threshold stress for crack healing of mullite reinforced by SiC whiskers and SiC particles and resultant fatigue strength at the healing temperature
K Takahashi, K Uchiide, Y Kimura, W Nakao, K Ando, M Yokouchi
Journal of the American Ceramic Society 90 (7), 2159-2164, 2007
302007
Single crystalline AlN film formed by direct nitridation of sapphire using aluminum oxynitride buffer
W Nakao, H Fukuyama
Journal of crystal growth 259 (3), 302-308, 2003