Recovery of mechanical strength by surface crack disappearance via thermal oxidation for nano-Ni/Al2O3 hybrid materials D Maruoka, M Nanko Ceramics International 39 (3), 3221-3229, 2013 | 52 | 2013 |
Crack disappearance by high-temperature oxidation of alumina toughened by Ni nano-particles AL Salas-Villaseñor, J Lemus-Ruiz, M Nanko, D Maruoka Advanced Materials Research 68, 34-43, 2009 | 32 | 2009 |
Effect of hydrogen concentration in reducing gas on the changes in mineral phases during reduction of iron ore sinter T Murakami, H Wakabayashi, D Maruoka, E Kasai ISIJ International 60 (12), 2678-2685, 2020 | 27 | 2020 |
Influences of Al2O3 grain size on high-temperature oxidation of nano-Ni/Al2O3 composites HV Pham, D Maruoka, M Nanko Journal of Asian Ceramic Societies 4 (1), 120-123, 2016 | 26 | 2016 |
Influence of Si-doping of nano-Ni dispersed Al2O3 composites on high-temperature oxidation D Maruoka, M Nanko Materials transactions 51 (9), 1570-1573, 2010 | 18 | 2010 |
Improved Crack Healing and High‐Temperature Oxidation Resistance of Ni/Al2O3 by Y or Si Doping D Maruoka, M Nanko Journal of the American Ceramic Society 99 (7), 2451-2457, 2016 | 17 | 2016 |
Crack Healing of Nano-Ni/Al2O3 Hybrid Materials via High-Temperature Oxidation D Maruoka, M Nanko Materials Science Forum 696, 378-383, 2011 | 15 | 2011 |
Recovery of mechanical property on nano-Co particles dispersed Al2O3 via high-temperature oxidation D Maruoka, T Itaya, T Misaki, M Nanko Materials transactions 53 (10), 1816-1821, 2012 | 14 | 2012 |
Crack-healing effectiveness of nano Ni+ SiC Co-dispersed alumina hybrid materials D Maruoka, Y Sato, M Nanko Advanced Materials Research 89, 365-370, 2010 | 13 | 2010 |
Morphology change and carburization characteristic of iron ore-coal composite during reduction under a simulated condition of blast furnace TY Huang, D Maruoka, T Murakami, E Kasai ISIJ International 59 (11), 1982-1990, 2019 | 12 | 2019 |
High‐Temperature Oxidation of Y2O3‐Doped Al2O3 Matrix Composites Dispersed with Nano‐Ni Particles M Nanko, D Maruoka, Y Sato International Journal of Applied Ceramic Technology 9 (1), 172-177, 2012 | 12 | 2012 |
Effect of types of carbonaceous material and CaO addition on reduction behavior of pre-reduced iron ore–carbon composite T Murakami, H Shinomiya, D Maruoka, E Kasai ISIJ International 59 (6), 1011-1017, 2019 | 9 | 2019 |
Advanced Ceramic Composite Using Self‐Healing and Fiber‐Reinforcement W Nakao, D Maruoka, S Ozaki, M Nanko, T Osada Mechanical Properties and Performance of Engineering Ceramics and Composites …, 2014 | 9 | 2014 |
Effect of ore type and gangue content on carburization and melting behavior of carbon-iron ore composite R Higashi, K Owaki, D Maruoka, T Murakami, E Kasai ISIJ International 61 (6), 1808-1813, 2021 | 7 | 2021 |
Reduction of Iron Ore by Uncarbonized Biomass in a Rotary Kiln Type Furnace T Murakami, R Higashi, D Maruoka, E Kasai ISIJ International 61 (12), 2971-2978, 2021 | 5 | 2021 |
Development of manufacturing principle of porous iron by carbothermic reduction of composite of hematite and biomass char T Murakami, T Takahashi, S Fuji, D Maruoka, E Kasai Materials transactions 58 (12), 1742-1748, 2017 | 5 | 2017 |
Rapid carbonization process using heat storage materials and characterization of the obtained char D Maruoka, T Nakamura, T Murakami, E Kasai Tetsu-To-Hagane/Journal of the Iron and Steel Institute of Japan 102 (12 …, 2016 | 5 | 2016 |
Effects of iron ore type and gangue mineral components on strength of sintered fine powder granule T MurakaMi, S NakaMura, D Maruoka, E Kasai Tetsu-To-Hagane/Journal of the Iron and Steel Institute of Japan 107 (6 …, 2021 | 4 | 2021 |
Influence of heat treatment temperature on self-healing effect of fe particle/Mullite ceramic composites D Maruoka, T Murakami, E Kasai Tetsu-To-Hagane/Journal of the Iron and Steel Institute of Japan 106 (11 …, 2020 | 4 | 2020 |
Crack-healing function of metal/Al2O3 hybrid materials M Nanko, D Maruoka, TD Nguyen IOP Conference Series: Materials Science and Engineering 18 (8), 082005, 2011 | 4 | 2011 |